Abstract

The method of this invention admixes in a high shear mixer 100 parts by weight of polydiorganosiloxane gum plasticizer chopped organic or inorganic fibers, and then when the fibers are uniformly mixed from 1 to 60 parts of reinforcing silica filler. The uniform mixture is then heated with mixing, under vacuum, optionally with nitrogen containing catalyst, to treat the filler and remove any volatiles, then cooled to give a uniform mixture with the fibers well dispersed throughout the mixture.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 6.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of producing a fiber reinforced silicone elastomer base consisting essentially of (A) admixing in a high shear mixer, (1) 100 parts by weight of a polydiorganosiloxane gum, (2) from 0.1 to 5.0 parts by weight of polydiorganosiloxane plasticizer per 10 parts by weight of filler (4), (3) chopped organic or inorganic reinforcing fibers, and when the above is uniformly mixed, (4) from 1 to 60 parts by weight of reinforcing silica filler, and then (B) optionally adding a small amount of a nitrogen containing catalyst and (C) heating with mixing under vacuum to treat the filler

  2. Claim 2Depends on #1

    The method of claim 1 in which the polydiorganosiloxane gum is at least 50 percent methyl radicals and has a viscosity of greater than 1000 Pa.s at 25° C.