Patents
US 4,640,901 A#3136851 Most CitedExpiredUnited States (USPTO)Utility

High temperature membrane

24Forward Citations (#3136851 Global)
0.6/yrCitation Velocity (#12756743 Global)
7.59Citation PageRank (#1676408 Global)
4Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The present invention concerns a method of making a silica-based membrane comprising the steps of: (1) pyrolyzing the material made of one of the class comprising polysilicone rubber, polysilane and polysiloxane at a temperature range of about 500 DEG C. to about 1000 DEG C. for about 2 hours (minimum) in an inert atmosphere; and (2) oxidizing the pyrolyzed material at a sufficient temperature range of about 300 DEG C. to about 1000 DEG C. to crosslink the material with oxygen. The membrane typically has a B.E.T. surface-area measurement of about 220 m2/g which indicates a highly porous membrane-about 40 to 70% porosity. The present invention may also be characterized by producing a pyrolyzed membrane by the method described above, and coating the membrane with silicon material to fill in the large micropores, and repyrolyzing the coated membrane to produce a membrane having extremely small micropores to assure that such gases as hydrogen and helium can be separated by the membrane product of the present invention to a high level of selectivity.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 24.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of forming a membrane capable of withstanding high temperatures for separating gases comprising the steps of: (1) pyrolyzing a silicon-based material having hydrocarbons and SiO chains in its structure to drive off substantially all hydrocarbons, said pyrolyzed silicon-based material consisting essentially of loosely connected SiO chains, said pyrolyzing being conducted at a temperature range of from about 500° C. to about 1000° C., for a minimum duration of about 2 hours, in an inert gaseous atmosphere under positive pressure; and (2) oxidizing said pyrolyzed silicon-based material

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗