Patents
US 4,632,701 A#1781164 Most CitedExpiredUnited States (USPTO)Utility

Process for the recovery of silver from a residue essentially free of elemental sulphur

35Forward Citations (#1781164 Global)
0.9/yrCitation Velocity (#8151025 Global)
3.90Citation PageRank (#4970796 Global)
7Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A process for the recovery of silver from a residue essentially free of elemental sulphur obtained by acidic pressure oxidation leaching or iron-containing sulphidic material which comprises forming a slurry of the residue with lime at a temperature of at least about 80° C. to raise the pH of the slurry to at least about 9. The slurry is maintained at this temperature for from about 0.5 to about 4 hours, and the resultant slurry is subjected to silver recovery treatment.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 35.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A process for the recovery of silver from a residue essentially free of elemental sulphur obtained by acidic pressure oxidation leaching of iron-containing sulphidic material, said residue containing less than about 10% by weight of elemental sulphur compared to the sulphur in the sulphidic material, comprising forming a slurry of the residue with lime at a temperature of at least about 80° C. to raise the pH of the slurry to at least about 9, maintaining the slurry at said temperature for from about 0.5 to about 4 hours, and subjecting the resultant slurry to silver recovery treatment.

  2. Claim 2Depends on #1

    A process according to claim 1 wherein the residue is silver and gold containing residue essentially free of elemental sulphur obtained by acidic pressure oxidation of refractory a

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗