Wear-resistant member for use in internal combustion engine and method for producing the same
Abstract
A wear-resistant member and method for producing the same which member may form a movable member in an internal combustion engine which is subjected to high pressure such as a rocker arm, tappet, cam, valve or valve seat. The member is formed as a combination of a ferrous sintered body and a ferrous base body having a common surface. The sintered body is formed from a compressed powder body disposed in contact with the ferrous base body. The powder body, in a preferred embodiment, consists of 0.5 to 7.0% by weight carbon, 0.1 to 5.0% phosphorus, the balance being iron, and having a porosity of 12 to 20% by volume at least 40% of which is pores having a pore size of not more than 300μ. The combined powder body and ferrous base body are heated to a temperature higher than the liquid-phase temperature of the powder body but lower than the melting point of the ferrous body to sinter the powder body.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 27.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for producing a wear-resistant member formed of a combination of a ferrous sintered body and a ferrous base body for use in an internal combustion engine comprising the steps of: (a) compressing a ferrous powder mixture to provide a compressed powder body, said compressed body consisting of 0.5 to 7.0% by weight carbon, 0.1 to 5.0% by weight phosphorus, 8.0 to 30.0% by weight chromium, not more than 10% by weight of at least one material selected from the group consisting of nickel, copper, cobalt, tungsten and molybdenum, and the balance being iron, and having a porosity of 12 to 20%
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗