Process for depositing a low resistivity tungsten silicon composite film on a substrate
Abstract
A composite film is provided which has a first layer of WSi x , where x is greater than 2, over which is disposed a second layer of a tungsten complex consisting substantially of tungsten with a small amount of silicon therein, typically less than 5%. Both layers are deposited in situ in a cold wall chemical vapor deposition chamber at a substrate temperature of between 500° and 550° C. Before initiating the deposition process for these first and second layers, the substrate onto which they are to be deposited is first plasma etched with NF 3 as the reactant gas, then with H 2 as the reactant gas, both steps being performed at approximately 100 to 200 volts self-bias. WSi x is then deposited onto the surface of the substrate using a gas flow rate for silane which is 20 to 80 times the flow rate of tungsten silicide, followed by deposition of a tungsten complex as the second layer, using a gas flow rate for tungsten hexafluoride which is 1 to 3 times the flow rate of silane, and a gas flow rate of hydrogen which is about 10 times the flow rate of silane. Similarly, in another embodiment, the tungsten complex without the silicide layer is deposited directly onto a silicon surface usi
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 83.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
In a chemical vapor deposition reactor having a vacuum housing, a process for depositing a composite film on a substrate comprising the steps of: a. plasma etching the substrate; b. after step a., depositing a first layer of WSi x over the substrate, with x being greater than or equal to 2; and c. depositing over the first layer a second layer of a tungsten and silicon complex having a percentage of silicon of less than 5% by weight.
- Claim 2Depends on #1
A process as in claim 1 wherein step a. includes: d. plasma etching the substrate using NF 3 as an etchant gas; and e. after step d. plasma etching the substrate using H 2 as an etchant gas.
- Claim 3Depends on #2
A process as in claim 2 wherein step b. includes: f. providing a flow of silane and tungsten hexafluoride into the vacuum housing, with the rate of flow of silane being 20 to
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (15 of 83 total)
References Cited — Backward Prior Art (6)
Non-Patent Literature (5)
- Akitmoto et al, "Formation of Wx Si-x by Plasma CVD," Appl. Phys. Lett., vol. 39, No. 5, Sep. 1981, pp. 445-447.
- Akitmoto et al, Formation of W x Si x by Plasma CVD, Appl. Phys. Lett., vol. 39, No. 5, Sep. 1981, pp. 445 447.
- Tang et al, "Plasma-Enhanced Deposition of Tungsten, Molybdenum, and Tungsten Silicide Film," Solid State Technology, Mar. 1983, pp. 125-128.
- Tang et al, Plasma Enhanced Deposition of Tungsten, Molybdenum, and Tungsten Silicide Film, Solid State Technology, Mar. 1983, pp. 125 128.
- Tsai et al, "Properties of Tungsten Silicide Film on Polycrystalline Silicon," J. Appl. Phys., vol. 52, No. 8, Aug. 1981, pp. 5350-5355.