Patents
US 4,617,366 A#4968884 Most CitedExpiredUnited States (USPTO)Utility

Process for manufacturing ethylene terpolymers and ethylene copolymers

18Forward Citations (#4968884 Global)
0.5/yrCitation Velocity (#17899290 Global)
2.74Citation PageRank (#8779221 Global)
2Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A process for the manufacture of radical ethylene terpolymers or copolymers comprising moieties derived from an alkyl (meth)acrylate and/or moieties derived from maleic anhydride by copolymerizing, in the presence of at least one free-radical initiator, a mixture of ethylene, (meth)acrylate and/or maleic anhydride in a device incorporating a primary compressor, the delivery pressure of which is between 200 and 300 bars, connected to a secondary compressor which is connected directly to a polymerization reactor, fresh ethylene being fed at the intake of the said primary compressor and said copolymerization being carried out in the said polymerization reactor under a pressure of between 1,000 and 2,500 bars and a temperature of between 140° and 280° C., wherein at least one the alkyl (meth)acrylate and/or maleic anhydride is fed directly into the said polymerization reactor. The process of the invention has the advantage of not requiring a homogenization device before the entry of the monomers into the reactor.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 18.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for the manufacture of radical ethylene terpolymers comprising 50 to 99.2% by weight of moieties derived from ethylene, 0.5 to 40% by weight of moieties derived from an alkyl (meth)acrylate and 0.3 to 10% by weight of moieties derived from maleic anhydride by copolymerizing, in the presence of at least one free-radical initiator, a mixture of ethylene, an alkyl (meth)acrylate and maleic anhydride, in a device comprising a primary compressor, the delivery pressure of which is between 200 and 300 bars, connected to a secondary compressor which is connected directly to a polymerization

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 18 total)

PatentTitleYearCitations
US 5,571,878 AEthylene-alkyl acrylate copolymers and derivatives having improved melt-point temperatures and adhesive strength and processes for preparing same199613
US 11,267,960 B2Impervious breathable ethylene copolymer film20220
US 6,509,424 B1Process for the preparation of ethylene copolymers, and their use as additives to mineral oil and mineral oil distillates200329
US 5,075,382 AAdhesive for glass laminate comprising silane-modified ethylene copolymer199116
US 6,762,253 B2Process for the preparation of ethylene copolymers, and their use as additives to mineral oil and mineral oil distillates20040
US 7,801,404 B2Optical cable and optical unit comprised therein20107
US 8,653,192 B2Method for manufacturing a polyester composition having improved impact properties20140
CN 116,515,029 AOlefin functional polymer and synthetic method and application thereof—0
US 8,642,703 B2Polyhydroalkanoate composition exhibiting improved impact resistance20140
US 5,543,477 ACopolymers of ethylene and alkyl acrylate with improved melt-point temperatures199636
US 9,212,265 B2Master mixture composition including a peroxide20150
US 11,292,896 B2Reinforced rubber composition20220
CN 116,715,792 AMethod for preparing glass fiber impregnating compound based on multi-olefin functional polymer—0
US 5,191,050 AFunctionalized ethylene polymers useful for metal coating, and process for their preparation19939
WO 2018/047864 A1Sealing material, production method therefor, and coating composition for sealing material—0

References Cited — Backward Prior Art (2)