Method for polymerizing bis(allyl carbonate) resin
Abstract
Fully cured, intact, solid castings of bis(allyl carbonate) resin, e.g., diethylene glycol bis(allyl carbonate), are prepared by polymerizing the resin with between about 0.75 and about 1.50 parts, per hundred parts of resin, of a monoperoxycarbonate, e.g., tertiarybutylperoxy isopropyl carbonate. An adhesion reducing amount, e.g., between about 25 and about 75 parts, per million parts of resin, of a mold release agent is incorporated into the liquid resin monomer to avoid cracking of the casting. Use of a mold release agent is not required when the resin is prepolymerized to about 15-50 percent allylic utilization.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 44.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
In the method of polymerizing polyol(allyl carbonate) monomer represented by the graphic formula, ##STR15## wherein R o is hydrogen, halogen or C 1 -C 4 alkyl, and n is a whole number from 1 to 3, wherein the monomer is mixed with peroxide initiator and the resultant mixture exposed to a thermal zone to polymerize the monomer, the improvement which comprises polymerizing a mixture of said monomer and an adhesion reducing amount of monomer-compatible mold release agent with, as the sole initiator, from about 0.75 to about 1.50 parts, per hundred parts of monomer, of monoperoxycarbonate repre
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗