Phenol-HCHO-resorcinol resins for use in forming fast curing wood laminating adhesives
Abstract
A phenol-resorcinol-formaldehyde resin and a method for making the same. In this method phenol and formaldehyde at an initial pH of 8.5 to 9.2 are reacted in the presence of a sodium sulfite catalyst. The reaction mixture is heated and refluxed until it has a viscosity of u-v on the Gardner bubble test. Additional resorcinol is added to the mixture and refluxing is continued until it has a viscosity of 30 to 100 Garner sections. The reaction mixture is diluted with a water miscible solvent to obtain a resin solution having a solids content of about 40 to 60 percent by weight and a viscosity of 2.0 to 3.5 poise. An alkali metal carbonate material in the amount of 4 to 8 percent by weight of the resin is added to make adhesives including this resin fast curing. Fumed silica is also added to the resin solution by means of high shear apparatus to make the solution thixotropic.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 41.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for making a soluble, fusible phenol-resorcinol-formaldehyde resin solution, which resin comprises about 50 to 95 moles phenol with about 5 to 50 moles resorcinol per 100 moles of total phenol and resorcinol and about 0.55 to 0.75 moles of formaldehyde for each mole total of phenol and resorcinol, said resin being prepared by the steps comprising: (a) reacting said phenol and said formaldehyde at an initial pH of from about 8.5 to 9.2 in the presence of a sodium sulfite catalyst in an amount of about 0.04 to 0.09 mole per mole of formaldehyde; (b) then heating the reaction mixture t
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗