Patents
US 4,606,808 A#8132201 Most CitedExpiredUnited States (USPTO)Utility

Method for the preparation of pitches for spinning carbon fibers

12Forward Citations (#8132201 Global)
0.3/yrCitation Velocity (#25428691 Global)
3.03Citation PageRank (#7439005 Global)
17Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The invention provides a method for the preparation of a pitch spinnable into pitch filaments as a precursor of carbon fibers starting from a pitch material such as coal tar and coal tar pitch. Different from the conventional procedure involving hydrogenation of the starting pitch, the starting pitch in the inventive method is first heated together with an aromatic oil, preferably, in the presence of a cracking catalyst such as silica-alumina and zeolite at 350° to 500° C. for 10 to 60 minutes under no pressurization with hydrogen and, after removal of insoluble materials, then heated at a temperature of 430° to 600° C. The thus obtained pitch for spinning has good spinnability and the carbon fibers prepared from the pitch have a unique microscopic structure and excellent physical properties exceeding by far the conventional pitch-based carbon fibers and approximating the HP-grade carbon fibers prepared from polyacrylonitrile fibers.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 12.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for the preparation of a pitch spinnable into a pitch filament which comprises as a first step heating a mixture of a coal tar or a coal tar pitch and an aromatic oil in the presence of a cracking catalyst at a temperature from 350° to 500° C. for from 10 to 60 minutes in a closed vessel under a spontaneously produced pressure, and as a second step removing insoluble materials from the mixture and heating the mixture at a temperature in the range from 430° to 600° C. under atmospheric pressure or under reduced pressure in an inert atmosphere.

  2. Claim 2Depends on #1

    The method as claimed in claim 1 wherein the aromatic oil is a distilled oil of coal tar or a light oil which is a byproduct in the thermal cracking of naphtha.

  3. Claim 3Depends on #1

    The method as claimed in claim 1 wherein the amount of the aromatic oil is in the range from 50 to

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗