Abstract

Herein disclosed is a process for producing a steel bar or steel wire having an improved structure of spheroidal cementite. The process is characterized in that a finish rolling is conducted within a temperature range between Ar1 and Ar3 or Arcm with a reduction ratio of at least 20%. The cooling rate of the steel before the finish rolling should be controlled in the following manner: When the hardenability of the steel is not higher than that of 0.15% C plain carbon steel, it is preferable to cool the steel at a cooling rate higher than 250 DEG C./sec. When the hardenability of the steel is between those of 0.15% to 0.4% C plain carbon steel, it is preferable to cool the steel at a cooling rate higher than 10 DEG C./sec. When the hardenability of the steel is not lower than that of 0.4% C plain carbon steel, it is preferable to cool the steel at a cooling rate higher than 2 DEG C./sec. The annealing may be conducted on the same production line as the hot working of the steel for a shorter time duration by an isothermal treatment, slow cooling treatment or repeating treatment. The annealing may be conducted also by a usual annealing method.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 12.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    Process for producing a steel bar or steel wire, which comprises: heating a steel containing less than 2% of C at a temperature higher than the Ac 1 point of the steel; rough working the heated steel; finish working the rough-worked steel within a temperature range between Ar 1 and Ar 3 or Arcm with a reduction ratio of at least 20%; and cooling the finish-worked steel at a cooling rate of lower than 60° C./minute to a temperature lower than 500° C.; thereby providing a steel bar or steel wire having a spheroidal cememtite structure.

  2. Claim 2Depends on #1

    Process as claimed in claim 1, wherein the steel is a plain carbon steel containing not higher than 0.15% of C or a low alloy steel having a hardenability not higher than that of 0.15% C plain carbon steel, and further comprising a step of: cooling the rough-worked steel at a cooling rate higher