Polyethylene superthin film and a process for the production of the same
Abstract
A polyethylene superthin film having a thickness of at most 3 μm, a tensile modulus of at least 2000 kg/cm 2 , a breaking strength of at least 500 kg/cm 2 and a haze of at most 10% is produced by heating and dissolving polyethylene having a weight average molecular weight of at least 5×10 5 in a solvent, forming a gel sheet from the resulting solution, subjecting the gel sheet to a solvent removal treatment to adjust the amount of the solvent in the gel sheet to 10 to 80% by weight, heating and stretching the sheet, removing the residual solvent therefrom and then subjecting the stretched product to a compressing treatment at a temperature of at most the melting point of the polyethylene.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 34.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A polyethylene superthin film consisting of polyethylene having a weight average molecular weight of at least 5×10 5 , and having a thickness of at most 3 μm, a tensile modulus of at least 2000 kg/cm 2 , a breaking strength of at least 500 kg/cm 2 and a haze of at most 10%.
- Claim 2Depends on #1
The polyethylene superthin film of claim 1, wherein the thickness is 0.1 to 1 μm, the tensile modulus is at least 4000 kg/cm 2 , the breaking strength is at least 1000 kg/cm 2 and the haze is at most 5%.
- Claim 3Depends on #1
The polyethylene superthin film of claim 1, wherein the weight average molecular weight is 1×10 6 to 10×10 6 .