Abstract
An optically black coating with improved infrared absorption is disclosed along with a process for formation therefor. An anodizable substrate is first treated in a surface modification step prior to anodizing to produce major surface modifications at least about 100 microns in width and at least about 50 microns in depth. Preferably, the depth is at least about 1/2 the width, and the modifications are present in a random series of irregularly sized modifications having widths from about 100 microns to about 1,000 microns and depths from about 50 microns to about 750 microns. A second aspect involves the use of steam for sealing the anodized surface.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 19 · Forward citations: 0.
Claims (10)
- Claim 1Independent Claim
In a process of making an object having a surface with improved capability for absorbing and reducing specular reflectance of infrared radiation having a wavelength greater than about 1 micron comprising the steps of anodizing an object composed of an anodizable metal to provide an anodized surface on the object, dying and sealing the anodized surface, the improvement comprising modifying the surface structure prior to anodizing to produce a series of major surface modifications at least about 100 microns in width and at least about 50 microns in depth.
- Claim 2Depends on #1
A process as claimed in claim 1 wherein the depth of said major surface modifications is at least about 1/2 the width thereof.
- Claim 3Depends on #1
A process as claimed in claim 1 wherein the major surface modifications form a random series of modifications from about 100 microns to about 1,000 microns wide and from about 50 microns to about 750 microns deep.
- Claim 4Depends on #1
A process as claimed in claim 1 wherein the major surface modifications are produced by photoetching.
- Claim 5Independent Claim
A process of making an object having a surface for absorbing infrared radiation and for reducing specular reflectance of infrared radiation comprising the steps of anodizing an object composed of an anodizable metal to provide an anodized surface on the object, dyeing the anodized surface, and reducing reflectance and improving resistance to atomic oxygen attack by sealing the anodized surface by contacting the surface with steam under a pressure of about 15 psig for about 30 minutes.
- Claim 6Independent Claim
A process of making an object having a surface with improved capability for absorbing and reducing specular reflectance of electromagnetic radiation having a wavelength greater than about 1 micron comprising the steps of anodizing an object composed of an anodizable metal to provide an anodized surface on the object, dying and sealing the anodized surface, the improvement comprising modifying the surface structure prior to anodizing to produce a series of major surface modifications at least about 100 microns in width and about 50 microns in depth, and reducing reflectance and improving resistance to atomic oxygen attack by sealing the anodized surface by contacting the surface with steam under pressure for at least about 2 minutes.
- Claim 7Depends on #6
A process as claimed in claim 6 wherein the depth of said major surface modifications is at least about 1/2 the width thereof.
- Claim 8Depends on #6
A process as claimed in claim 6 wherein the major surface modifications form a random series of modifications from about 100 microns to about 1,000 microns wide and from about 50 microns to about 750 microns deep.
- Claim 9Depends on #6
A process as claimed in claim 6 wherein the major surface modifications are produced by photoetching.
- Claim 10Depends on #6
A process as claimed in claim 6 wherein the pressure is about 15 psig and the sealing time is about 30 minutes.
Technical Overview & Description
FIELD OF INVENTION The present invention relates to a body having a surface which has the property of extremely low specular and diffuse reflectance of electromagnetic radiation therefrom, and with improved absorption in the infrared region. The invention also relates to methods of manufacturing such a body. PRIOR ART A variety of coatings are known for optical applications wherein it is sought to maximize absorption and minimize specular reflectance of light or electromagnetic radiation from the surface thereof. One such optically black coating using anodized aluminum is disclosed in Wade et al. U.S. Pat. No. 4,111,762. Optically black coatings are of particular interest for use in connection with infrared instruments. In previous practice, thick black paints and anodized coatings, such as disclosed in U.S. Pat. No 4,111,762, have been used to coat surfaces in infrared instruments. However, both of those methods have certain limitations. Black paints have a tendency to crack or separate from the metal substrate under thermal cycling conditions. Since many infrared instruments operate at liquid helium temperatures and undergo many thermal cycles, paint separation can be a significant problem. For increased absorption at longer wavelengths, thicker layers of paint are needed. An increase in the paint thickness aggravates the cracking or separation problem. Additionally, paints outgas losing up to 10% by weight after vacuum exposure. Some of the chemicals which outgas can be highly corrosive to microelectronic components. Furthermore, in a cryogenically cooled optical system, outgassed chemicals may condense onto cooled optical surfaces. Moreover, most infrared absorbing paints contain carbon black and recent experiments have shown that carbon black reacts with the five electron volt atomic oxygen prevalent at low earth orbits. The anodized optically black surface produced in accordance with U.S. Pat. No. 4,111,762 eliminates the co
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (19)
| Patent | Title | Year | Citations |
|---|
Non-Patent Literature (2)
- "Preliminary Performance Data on an Improved Optical Black for Infrared Use," Pompea et al., Proc. Society of Photo-Optical Instrumentation Engineers, vol. 400, New Optical Materials (1983), 128.
- Preliminary Performance Data on an Improved Optical Black for Infrared Use, Pompea et al., Proc. Society of Photo Optical Instrumentation Engineers, vol. 400, New Optical Materials (1983), 128.