Ethylene copolymer compositions for rotational molding
Abstract
Provided is an ethylene copolymer composition for rotational molding, comprising a copolymer of a predominant ethylene and 0.02 to 1 mole % of a non-conjugated diene represented by the following formula (I) or (II) or a derivative thereof: <IMAGE> (I) <IMAGE> (II) wherein R1 is an alkylene group having one or two carbon atoms and R2 is hydrogen or an alkyl group having one or two carbon atoms, and an organic peroxide, said copolymer having a melt index of 2 to 50 g/10 min, a density of 0.930 to 0.970 g/cm3 and a maximum peak temperature (Tm) measured according to Differential Scanning Calorimetry (DSC) of not lower than 100 DEG C.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 13.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
An ethylene copolymer composition for rotational molding, comprising a copolymer of ethylene, 0-3 mole % of an α-olefin and 0.02 to 1% of a non-conjugated diene represented by the following formula (I) or (II) or a derivative thereof: ##STR3## wherein R 1 is an alkylene group having one or two carbon atoms and R 2 is hydrogen or an alkyl group having one or two carbon atoms, and an organic peroxide, said copolymer having a melt index of 2 to 50 g/10 min, a density of 0.930 to 0.970 g/cm 3 and a maximum peak temperature (Tm) measured according to Differential Scanning Calorimetry (DSC) of no
- Claim 2Depends on #1
An ethylene copolymer composition for rotational molding as claimed in claim 1, wherein said non-conjugated diene is 5-vinyl-2-norbornene.
- Claim 3Independent Claim
An ethylene copolymer composition for rotational molding
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗