Patents
US 4,587,283 A#1647870 Most CitedExpiredUnited States (USPTO)Utility

Cement slurries for deep holes, with a copolymer content for reducing the water loss

36Forward Citations (#1647870 Global)
0.9/yrCitation Velocity (#7902589 Global)
9.63Citation PageRank (#1129216 Global)
11Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Cement slurries for deep holes, with a content of copolymers which are composed of 5-95% by weight of groups of the formula ##STR1## in which R 1 is hydrogen or methyl, R 2 is C 2 -C 10 -alkylene and Me is ammonium, lithium, sodium or potassium, of 5-60% by weight of groups of the formula ##STR2## in which R 3 is hydrogen, --CH 3 or C 2 H 5 and R 4 is --CH 3 or C 2 H 5 , or R 3 and R 4 together are a propylene group which, with incorporation of the radical ##STR3## forms a pyrrolidone radical, and of 0-90% by weight of groups of the formula ##STR4## in which R 6 is hydrogen or methyl and R 7 is carboxamido, carboxyl, cyano or carbomethoxy. These copolymers reduce the water loss of cement slurries which are required for deep holes.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 36.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A cement slurry comprised of water and cement, which comprises a copolymer comprised of: (a) 10-80% by weight of groups of the formula ##STR9## in which R 1 is hydrogen or methyl, R 2 is C 2 -C 10 -alkylene and Me is ammonium, lithium, sodium or potassium; (b) 10-60% by weight of groups of the formula ##STR10## in which R 3 is hydrogen, --CH 3 or --C 2 H 5 and R 4 is --CH 3 or --C 2 H 5 ; and (c) 0-75% by weight of groups of the formula ##STR11## in which R 6 is hydrogen or methyl and R 7 is carboxamido, carboxyl, cyano or carbomethoxy.

  2. Claim 2Depends on #1

    A cement slurry as claimed in claim 1, which comprises a copolymer comprised of: (a) 30-80% by weight of groups of the formula I or II; (b) 10-30% by weight of groups of the formula III and (c) 10-50% by weight of groups of the formula IV.

  3. Claim 3Independent Claim

    A cement slur

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 36 total)

PatentTitleYearCitations
US 2007105995 A1Fluid loss control additives for foamed cement compositions and associated methods—2
US 10,822,917 B2Method of cementing a well using delayed hydratable polymeric viscosifying agents20200
US 2003159625 A1High temperature viscosifying and fluid loss controlling additives for well cements, well cement compositions and methods—11
US 2006272820 A1Cement compositions comprising environmentally compatible defoaming agents and methods of use—15
US 2010160488 A1Graft polymer mixture—23
US 5,153,240 AFluid loss additives for well cementing compositions containing a tetrapolymer199214
US 2007101905 A1Fluid loss control additives for foamed cement compositions and associated methods—9
US 2005075249 A1High temperature viscosifying and fluid loss controlling additives for well cements, well cement compositions and methods—8
US 4,674,574 AFluid loss agents for oil well cementing composition1987120
US 5,260,391 ATetrapolymerization product of 2-acrylamido-2-methyl propane sulfonic acid/associated salts, n-vinyl pyrrolidone, acrylamide, and acrylic acid/associated salts199312
US 5,988,279 AMethod for control of fluid loss and gas migration in well cementing199928
US 8,802,748 B2Graft polymer mixture20145
US 7,273,103 B2Cement compositions comprising environmentally compatible defoaming agents and methods of use20075
US 5,510,436 AWater-soluble copolymers useful in drilling fluids199635
US 5,109,042 AFluid loss additive for cement slurries containing a n-vinyl-2-pyrrolidone-ω-2-acrylamido-2-methylpropane sulfonate-ω-acrylic acid-ω-acrylamide polymer199241