Method of preparing coal to increase its calorific value and making it safe for storage and transport

1Forward Citations (#59483619 Global)
0.0/yrCitation Velocity (#58903693 Global)
0.77Citation PageRank (#59483619 Global)
14Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

There is described an improved method for treating low rank coal to lessen the risk of autogenous heating and attendant combustion hazards by means of passing the coal through a bath of molten metal to elevate its temperature into the range Td to Td+50° C., where Td is the temperature of decomposition of the coal.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 1.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of treating low-rank coal to lessen the risk of autogenous heating and attendant combustion hazards, comprising the step of passing said coal through a bath of molten metal to elevate the temperature of said coal into the range Td to Td+50° C., where Td is the decomposition temperature of said coal.

  2. Claim 2Depends on #1

    The method of claim 1 including the additional step of rapidly quenching the coal in a liquid medium, said heating of the coal causing the formation of volatile pyrolytic material in the pores thereof, said rapid quenching causing said pyrolytic materials to condense in said pores to form self-solidifying plugs therein which inhibit the entry of water, oxygen and like substances into said pores.

  3. Claim 3Independent Claim

    The method of cl

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗