Method of producing a polycrystalline transparent spinel sintered body
Abstract
The disclosed polycrystalline transparent sintered body contains Al 2 O 3 and MgO at a molar ratio of (0.54:0.46) to (0.58:0.42) and has in-line transmittance of more than 77% for 1 mm thickness at a light wavelength of 0.6 μm, which sintered body is produced by preparing fine spinel powder through hydrolysis of an isopropanol solution of aluminum isopropoxide and magnesium isopropoxide, forming a shaped body from the powder, and sintering the shaped body.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 27.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
A method of producing a polycrystalline transparent spinel sintered body, comprising the steps of preparing an isopropanol solution of aluminum isopropoxide and magnesium isopropoxide, generating precipitates by hydrolysis of the isopropanol solution, heating the precipitates so as to form fine spinel powder consisting essentially of Al 2 O 3 and MgO in a molar ratio of (0.502:0.498) to (0.524:0.476), forming a shaped body from the spinel powder, and firing the shaped body at a temperature higher than 1,700° C. in a hydrogen atmosphere.
- Claim 2Depends on #1
A method of producing a polycrystalline transparent spinel sintered body as set forth in claim 1, wherein said hydrolysis occurs at a temperature which is close to the boiling point of isopropanol.
- Claim 3Independent Claim
A method of producing a polycrystalline transparent spinel sintered sinter