Abstract

An alpha alumina monohydrate, AlO(OH), gel is produced which is capable of readily dispersing in aqueous solutions to yield a shear-rate thinning mixture. The alpha alumina monohydrate is made by reacting an acid reactant and a base reactant, wherein at least one contains aluminum, in an aqueous medium in proportions to yield a mixture having a pH of from about 7.5 to 10. The gel is treated to remove much of the by-product salts. One preferred method involves filtering the reaction product to remove the by-product salts and then further washing the filter cake with water. Upon dispersing the filter cake in water it yields a shear-rate thinning liquid having increased viscosifying power per unit weight of the AlO(OH) and this is measured as a higher K value in the rheological power model.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 8.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    In the method of making uncrystallized AlO(OH) gel for use in a drilling fluid by reacting an acid and a base, at least one of which contains an aluminum salt, to form a reaction product slurry comprising uncrystallized AlO(OH) and a by-product salt, the improvement comprising treating the reaction product to reduce the amount of by-product salt by filtering the reaction product slurry and water-washing the recovered filter cake so as to increase the viscosifying power of the AlO(OH) when dispersed in water as measured by a higher K in the power law model.

  2. Claim 2Depends on #1

    A process according to claim 1, wherein the washed filter cake is further dried to an AlO(OH) content of about 20 to about 25% by weight.

  3. Claim 3Depends on #1

    A process according to claim 1, wherein after the reaction product is formed it is maintained at ambient conditions

Technical Overview & Description