Bolting bar material and a method of producing the same
Abstract
A bolting bar material consists in weight ratio of 0.05˜0.2% of C, 0.05˜0.8% of Si, 0.8˜2% of Mn, not more than 0.035% of P, not more than 0.030% of S, 0.005˜0.05% of Nb, 0.01˜0.05% of Al, 0.005˜0.025% of N, 0.05˜0.35% in total of at least one element selected from not more than 0.25% of V, not more than 0.25% of Ti and not more than 0.25% of Zr, and if necessary, 0.05˜1.5% in total of at least one element selected from 0.05˜0.5% of Ni, 0.05˜0.5% of Cr and 0.05˜0.5% of Mo, and the balance of Fe. In the production of the bolting bar material, the steel having the above composition is heated to 1000°˜1100° C., rolled at a finish rolling temperature of 750°˜950° C. and cooled at a rate of 5°˜50° C./sec on average.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 12.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of producing a bolting bar material, characterized in that a steel material consisting of 0.05˜0.2% by weight of carbon, 0.05˜0.8% by weight of silicon, 0.8˜2% by weight of manganese, not more than 0.035% by weight of phosphorus, not more than 0.030% by weight of sulfur, 0.005˜0.05% by weight of niobium, 0.01˜0.05% by weight of aluminum, 0.005˜0.025% by weight of nitrogen, 0.05˜0.25% by weight of vanadium and the balance of iron is heated to 1000°˜1100° C. and then rolled at a finish rolling temperature of 750°˜950° C. and cooled at an average cooling rate of 5°˜50° C./sec during the
- Claim 2Independent Claim
A method of producing a bolting bar material, characterized in that a steel material consisting of 0.05˜0.2% by weight of carbon, 0.05˜0.8% by weight of silicon, 0.8˜2% by weight of manganese, not more than 0.035% by weight
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗