Patents
US 4,578,431 A#680331 Most CitedExpiredUnited States (USPTO)Utility

Process for improving melt strength of ethylene polymers by treatment with organic peroxide

59Forward Citations (#680331 Global)
1.5/yrCitation Velocity (#3640886 Global)
11.09Citation PageRank (#893143 Global)
13Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Melt strength of polyethylene and ethylene-higher olefin copolymers during processing is improved by pretreating the polymer in melt form at a temperature of at least 230 DEG C. in the presence of an organic peroxide for a period of time equal to at least three times the half-life of the organic peroxide at the melt temperature.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 59.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A process treating a film-forming copolymer of ethylene and an olefin having 4 to 8 carbons atoms, or of a high density ethylene homopolymer, comprising: heating said ethylene copolymer in melt form at a temperature of from about 230° C. to 340° C. in the presence of an effective amount of from 100 ppm to 2000 ppm of an organic peroxide for a period of time equal to at least three times the half-life of the organic peroxide at the heating temperature to increase the melt strength of said copolymer so that the copolymer is suitable for extrusion into a film by blown film extrusion.

  2. Claim 2Depends on #1

    The process of claim 1 in which said ethylene polymer is a copolymer of ethylene and an olefin having 4 to 8 carbon atoms and a density of 0.90 to 0.94.

  3. Claim 3Depends on #1

    The process of claim 1 in which said ethylene polymer is high density ethy

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗