Soluble additives to improve high temperature properties of alumina refractories
Abstract
A method for improving the high temperature properties of 42 to 70 percent by weight Al2O3 containing alumina refractories by adding thereto a soluble metal compound and firing to at least 1450 DEG C. for a time sufficient to convert the soluble metal compound to a refractory oxide or phase and for the refractory oxide or phase to react with the non-Al2O3 constituents of the refractory for preventing or reducing the presence or effect of detrimental compounds or phases on the high temperature properties of the refractory. The resulting relatively low Al2O3 content, porous, alumina refractory includes within its pores from 1 to 10% by weight of a refractory oxide or phase and is characterized by high temperature property values substantially greater than the corresponding values for the same refractory body without said refractory oxide or phase in its pores.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 24.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for improving the high temperature properties of relatively low Al 2 O 3 content alumina refractories comprising the steps of: providing a porous alumina refractory containing from 42 to 70 percent by weight Al 2 O 3 ; impregnating said refractory with a solution of a soluble compound, said compound containing an ion selected from the group consisting of chromium, mixtures of chromium and iron, zirconium, calcium, molybedenum and tungsten and being capable of conversion to a refractory oxide or phase on being heated to a temperature below the melting point of the alumina refract
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗