Patents
US 4,552,913 A#3706284 Most CitedExpiredUnited States (USPTO)Utility

One component polyurethane SMC surface coat

22Forward Citations (#3706284 Global)
0.5/yrCitation Velocity (#14704119 Global)
3.23Citation PageRank (#6736828 Global)
2Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A one component polyurethane precursor suitable as an in-mold coating composition composed of a prepolymer of an organic polyisocyanate with a polyol of a polyether polyol of 2 and 3 hydroxyl groups or a polyester polyol of 2 and 3 hydroxyl groups to give a free NCO content of about 3 to about 15% with a salt complex of a diamine, such as NaCl complex of MDA. The amount of filler and plasticizer, viz, those preferably of the crown or pseudocrown ethers preferably are adjusted to give the precursors a viscosity of about 5 to about 50 pascal seconds at the temperature the precursors are applied, but usually less than about 80° C. These precursors are spread, applied or preferably injected onto the surface of the fiberglass molding viz a polyester or epoxy resin one and pressed at a pressure of about 5 to 200 psi (34,475 to 1,379,000 pascals) and higher at a temperature of at least 80° C. to cure the precursor to give a polyurethane coating on the fiberglass molding.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 22.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of in-mold coating a molded shaped article composed of epoxy/glass fibers or vinyl ether/glass fibers comprising applying a stable one component polyurethane precursor comprising a polyurethane prepolymer having about 3 to 15% NCO by weight and a salt complex of a diamine to a shaped surface of the article closing the mold on the shaped article under a pressure of about 500 to 900 psi (34,475 to 1,379,000 pascals) and a temperature of at least 80° C. to spread the precursor over the surface of the shaped article and cure it, and open the mold to remove the polyurethane coated article.

  2. Claim 2Independent Claim

    An in-mold coating composition comprising a stable one component polyurethane precursor composed of a prepolymer of sufficient organic polyisocyanate and at least one polyol having a molecular weight of about 500 to 10,000 to give the prep

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 22 total)

PatentTitleYearCitations
EP 3,919,266 A1Honeycomb load structure with over mold—0
RU 2,434,028 C2Improved single-component polyurethane system stable during storage20110
US 6,893,683 B1Process for the preparation of a coating, a coated substrate, an adhesive, a film or sheet20056
NL 1,013,179 C2Werkwijze voor de bereiding van een coating, een gecoat substraat, plakmiddel, film of vel, een aldus verkregen product en bekledingsmengsel ten gebruike bij de werkwijze.20010
US 2007213497 A1Storage stable one component polyurethane system—13
US 2008164634 A1Methods of forming a door skin—2
US 11,465,379 B2Honeycomb load structure with over mold20221
EP 3,578,354 A1Honey comb structure with over mold—0
US 12,318,977 B2Method of manufacturing a load structure20250
WO 0,123,451 A3Process for the preparation of a coating, a coated substrate, an adhesive, a film or sheet, for the thus obtained products and the coating mixture to be used in the process—0
CN 101,495,529 BImproved storage stable one component polyurethane system20120
AU 775,340 B2Process for the preparation of a coating, a coated substrate, an adhesive, a film or sheet, for the thus obtained products and the coating mixture to be used in the process20040
EP 3,578,355 A1Method of manufacturing a load structure—1
KR 100,831,525 B1Process for the preparation of a coating, a coated substrate, an adhesive, a film or sheet, for the thus obtained products and the coating mixture to be used in the process20080
WO 2008/136788 A3Improved storage stable one component polyurethane system—0

References Cited — Backward Prior Art (2)