Patents
US 4,550,007 A#1589794 Most CitedExpiredUnited States (USPTO)Utility

Process for production of a plastic bottle

37Forward Citations (#1589794 Global)
0.9/yrCitation Velocity (#7905746 Global)
6.52Citation PageRank (#2153139 Global)
5Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A plastic bottle made of biaxially oriented polyethylene terephthalate comprises a narrow neck portion, a downwardly and outwardly flared shoulder portion continuous from the neck portion, a generally cylindrical body portion and a bottom portion, wherein said portions except for the neck portion have a density of at least 1.375, and the internal volume increase rate is less than 5% when the bottle filled with a liquid at 20 DEG C. containing a 2 gas volume of carbon dioxide gas is immersed in warm water at 75 DEG C. for 30 minutes.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 37.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for producing a plastic bottle wherein all portions except for the neck have substantially uniform thickness, a density of at least 1.379, and the internal volume increase rate is less than 3.4% when the bottle filled with a liquid at 20° C. containing a two gas volume of CO 2 is immersed in 75° C. water for 30 minutes, which comprises blow stretching a parison of polyethylene terephthalate in a first mold to form an intermediate product, transferring the intermediate product to a second mold while the intermediate product which has undergone shrinkage is still soft, and restretchin

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗