A method for strengthened porcelain tooth is disclosed, which comprises depositing one or more inorganic salts of metals selected from rubidium, cesium, and potassium on the surface of a porcelain tooth obtained by sintering a dental porcelain material containing feldspar as a main raw material and sodium, and heat treating the porcelain tooth at temperature of 380° C. or higher but lower than the melting point of the inorganic salt and the strain temperature of the porcelain tooth. According to the method of this invention, the porcelain tooth can be strengthened with ease while maintaining translucency and color tone as in a natural tooth, without using any special device.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 22.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for strengthening porcelain tooth comprising depositing one or more inorganic salts of metals selected from rubidium, cesium, and potassium on the surface of a porcelain tooth obtained by sintering a dental porcelain material containing feldspar as a main raw material and sodium, and heat treating the porcelain tooth at temperatures of 380° C. or higher but lower than the melting point of said inorganic salt and the strain temperature of said porcelain tooth.

  2. Claim 2Depends on #1

    A method for strengthening porcelain tooth as claimed in claim 1, wherein said porcelain tooth has a coefficient of thermal expansion of 15×10 -6 /°C. or less.

  3. Claim 3Independent Claim

    A method for strengthening porcelain tooth as claimed 1, wherein said porcelain tooth on which said inorganic salt of metal has been deposited is treated for from 5 minutes to 60 minu

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 22 total)

PatentTitleYearCitations
EP 4,335,430 A1Glass-ceramic dental prosthesis and method for preparing the same, method for reinforcing glass or glass-ceramics, and alkaline reinforcing paste—0
US 11,370,702 B2Method to increase the strength of a form body of a lithium silicate glass ceramic20221
US 11,427,504 B2Method to produce a dental structure and dental structure20220
CN 107,847,399 AIncrease the method for the intensity of lithium metasilicate glass ceramics formed body—4
CN 106,083,007 BMetal-porcelain color masking ceramic agent porcelain powder and preparation method thereof20170
US 2006117989 A1Uniformly coloured ceramic framework and colouring solution—29
EP 3,095,436 A1Method to increase the strength of a form body of lithium silicate glass ceramic—3
EP 3,095,434 A1Method to increase the strength of a form body of lithium silicate glass ceramic—3
US 2010062398 A1Colouring solution for dental ceramic framework and related methods—10
AU 2016267543 B2Method to increase the strength of a form body of lithium silicate glass ceramic20200
WO 2016/188914 A1Method to increase the strength of a form body of lithium silicate glass ceramic—6
US 10,745,319 B2Method to increase the strength of a form body of lithium silicate glass ceramic20200
WO 2016/188904 A1Method to increase the strength of a form body of lithium silicate glass ceramic—5
US 10,065,895 B2Colouring solution for dental ceramic articles and related methods20182
US 5,705,273 AMethod for strengthening dental restorative materials199827