Bath and process for high speed electroplating of palladium
Abstract
A palladium electroplating bath capable of plating highly ductile palladium metal. The bath comprises a palladium amine complex salt as a source of the palladium metal, ammonium sulfate, an ammonium halide, an alkali metal pyrophosphate, a stress reducing agent, and a minor amount of cyanide ions. In general, the cyanide ions are furnished to the bath by the addition of alkali metal cyanide. The pH of the bath will range from about 7 to 9. Electrolytic deposition will be carried out at a temperature of from about 50 to 80 degrees C. at high current densities up to about 3000 ASF. The method of depositing ductile palladium foil on a variety of substrates is also described and claimed.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 7.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
An improved bath for electroplating highly ductile palladium metal, said bath comprising from about 10 to 80 g/l of palladium metal in the form of a palladium amine complex; about 20 to 90 g/l of ammonium sulfate; about 10 to 80 g/l of ammonium halide; from about 20 to 150 g/l of an alkali metal pyrophosphate; a stress reducing agent; and a minor amount of cyanide ions.
- Claim 2Depends on #1
The bath of claim 1 which contains about 1 to 20 ppm of cyanide ions.
- Claim 3Depends on #1
The bath of claim 1 wherein the cyanide ions are in the form of an alkali metal cyanide.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (7 of 7 total)
References Cited — Backward Prior Art (2)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 2,452,308 A | Process of plating palladium and plating bath therefor | 1948 | 19 |
| US 4,098,656 A | Bright palladium electroplating baths | 1978 | 41 |