Blends of ionomer with propylene copolymer and articles

42Forward Citations (#1277280 Global)
1.0/yrCitation Velocity (#6163781 Global)
6.87Citation PageRank (#1972540 Global)
22Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Blends of (a) 80-93 weight percent of an ethylene/acid ionomer, and (b) 7-20 weight percent of a propylene/α-olefin copolymer are used to prepare peelable seals having nearly constant and predictable peel strength over an extended heat seal temperature range. Some of the seals so produced also show stress whitening.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 22 · Forward citations: 42.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    Coextrusions for producing film characterized by a nearly constant peel strength over an extended heat seal temperature range, made from a molecular blend of polymeric materials comprising: (a) 80-93 weight percent of an ethylene/acid ionomer, and (b) 7-20 weight percent of a propylene/α-olefin copolymer, wherein the α-olefin comprises 1-12 weight percent of the copolymer, and wherein said coextrusion further comprises at least one extrudable material other than said molecular blend.

  2. Claim 2Depends on #1

    Laminates made from the coextrusions of claim 1.

  3. Claim 3Independent Claim

    Laminates characterized by a nearly constant peel strength over an extended heat seal temperature range, made from a molecular blend of polymeric materials comprising: (a) 80-93 weight percent of an ethylene/acid ionomer, and (b) 7-20 weight percent of a propylene/α-olefin copolymer,