Patents
US 4,536,034 A#3688242 Most CitedExpiredUnited States (USPTO)Utility

Method for immobilizing contaminants in previously leached ores

22Forward Citations (#3688242 Global)
0.5/yrCitation Velocity (#14700109 Global)
3.46Citation PageRank (#6010975 Global)
6Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

This invention relates to a process for reducing to environmentally acceptable levels the amount of soluble or mobile contaminants in formations that have been subjected to in situ leaching to recover mineral values therefrom. The present process is also applicable to surface milling operations. In accordance with the present invention, an aqueous solution containing orthophosphates is introduced into the formation to immobilize contaminants by forming a relatively stable precipitate. For example, radionuclides such as uranium, thorium or radium form stable precipitates with orthophosphates. When the formation fluids contain a high concentration of carbonates, the formation fluids are treated to reduce the carbonates concentration to levels which do not substantially interfere with the phosphate precipitation of contaminants.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 22.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for restoring a subterranean formation subjected to oxidative leaching, excluding a carbonate leaching process, to environmentally acceptable levels of soluble contaminants by use of an aqueous restorative fluid comprising: (a) making said restorative fluid with sufficient phosphate ions therein and a pH value suitable for forming insoluble precipitates in said fluid with the ions of said soluble contaminants; and (b) injecting said restorative fluid into said formation in a volume sufficient to form an insoluble precipitate within said formation.

  2. Claim 2Depends on #1

    The method as recited in claim 1 where in step (b) at least one pore volume of said restorative fluid is injected into said formation.

  3. Claim 3Depends on #1

    The method as recited in claim 1 where in step (a) the restorative fluid contains from about 0.01 to about 1.0 gram

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 22 total)

Non-Patent Literature (2)

  • Yan, "Calcium Control in In-Situ Uranium Leaching Process", 11/80, pp. 2068-2073.
  • Yan, Calcium Control in In Situ Uranium Leaching Process , 11/80, pp. 2068 2073.