Nitride bonded oxide refractories
Abstract
This invention relates to a method for producing nitride bonded refractory shapes in which the bonding matrix is formed in situ. The method comprises forming a batch including a coarser portion selected from the group calcined and fused aggregates of alumina, aluminosilicate, and magnesium aluminate spinel and a finer portion consisting essentially of finely divided silicon metal and alumina as well as fines of the above mentioned refractory aggregate needed to achieve the desired screen analysis. The silicon metal and alumina react in the nitriding atmosphere to form a low porosity matrix generally comprising silicon oxynitride with corundum distributed therethrough.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 14.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A nitride bonded refractory shape formed by an in situ reaction in a nitriding atmosphere consisting essentially of a size graded batch comprising 55 to 63 percent, by weight, -3 to +65 mesh Tyler coarse refractory aggregate, selected from the group consisting of calcined and fused aggregates of alumina, alumino-silicate, and magnesium aluminate spinel, and 37 to 45 percent, by weight, of a -65 mesh Tyler, fine portion consisting essentially of 3 to 20 percent, by weight, silicon metal, 0.75 to 20 percent, by weight, alumina, and the balance consisting of fines of the refractory aggregate, the
- Claim 2Depends on #1
The shape of claim 1 wherein the refractory aggregate is substantially free of iron oxide, chrome oxide and lime.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗