Process for making tetrafluoroethylene fine powder
Abstract
Tetrafluoroethylene fine powder resins are made by adjusting temperature during polymerization wherein: (a) at the beginning of the polymerization the temperature is between 70°-90° C., (b) when between 5-30% of the total amount of tetrafluoroethylene has been polymerized, the temperature is raised to between 100°-125° C., (c) after 20-80% of the total tetrafluoroethylene has been polymerized and after step (b) has been carried out, the temperature is lowered by at least 30° C. from the temperature used in step (b).
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 13.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for polymerizing tetrafluoroethylene in an aqueous medium in the presence of a substantially non-telogenic anionic surfactant present in an amount which maintains colloidal particles of polymerization product in dispersed form, said process being carried out by reacting tetrafluoroethylene in said aqueous medium in the presence of at least one tetrafluoroethylene polymerization initiator wherein the temperature at which polymerization is carried out is varied as follows: (a) at the beginning of the polymerization the temperature is between 70°-90° C., (b) when between 5-30% of the
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗