Powder varnishes based on partially blocked isophorone diisocyanate isocyanurate and hydroxyl group containing polyester, and method for producing matte coatings
Abstract
A powder coating composition exhibiting good storage stability, having a particle size less than 100 microns and yielding a matte surface after hardening at a temperature of 170 DEG to 220 DEG C., comprising: a mixture of at least one hydroxyl group containing polyester, at least one isophorone diisocyanate isocyanurate partially blocked with epsilon -caprolactam having a melting point above 130 DEG C. and a free NCO content between 2 to 8 wt. % and additives.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 12.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A powder coating composition exhibiting good storage stability, having a particle size less than 100 microns and yielding a matte surface after hardening at a temperature of 170° to 220° C., comprising: a mixture of at least one hydroxyl group containing polyester, at least one isophorone diisocyanate isocyanurate partially blocked with ε-caprolactam having a melting point above 130° C. and a free NCO content between 2 to 8 wt. % and additives.
- Claim 2Depends on #1
The composition of claim 1, wherein the free NCO content of said blocked isocyanurate is 3 to 7 wt.%.
- Claim 3Depends on #1
The composition of claim 1, wherein said partially blocked isophorone isocyanurate is prepared by reacting IPDI-isocyanurate with ε-caprolactam in amounts such that the NCO/NH ratio of the reactants is 1:X, wh