Method of manufacturing austenitic stainless steel plates

14Forward Citations (#6900362 Global)
0.3/yrCitation Velocity (#22525132 Global)
2.61Citation PageRank (#9455474 Global)
3Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

An austenitic stainless steel plate containing up to 0.08 wt. % of carbon, up to 1.0 wt. % of silicon, up to 2.0 wt. % of manganese, 8.0-16.0 wt. % of nickel, 16.0-20.0 wt. % of chromium, 0-30 wt. % of molybdenum, up to 0.25 wt. % of nitrogen and the balance of iron and inherent impurities, is manufactured by rolling a stainless steel blank at a temperature higher than TR( DEG C.)=940+30(%Mo), and then cooling the rolled blank from a temperature above 800 DEG C. to a temperature below 500 DEG C. at a cooling speed higher than Rc ( DEG C./sec.) shown by the following equations: log (Rc)=-0.32+14(%C+%N)-0.067(%Mo) when (%C+%N)</=1.0 wt. %; and log (Rc)=1.08-0.067(%Mo) when (%C+%N)>1.0 wt. %.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 14.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of manufacturing austenitic stainless steel plates containing up to 0.08 wt. % of carbon, up to 1.0 wt. % of silicon, up to 2.0 wt. % of manganese, 8.0-16.0 Wt. % of nickel, 16.0-20.0 wt. % of chromium, 0-30 wt. % of molybdenum, up to 0.25 wt. % of nitrogen and the balance of iron and inherent impurities, the method comprising the steps of: rolling a stainless steel blank at a temperature higher than T R =940+30 (% Mo); and then cooling the rolled blank from a temperature above 800° C. to a temperature below 500° C. at a cooling speed higher than Rc (°C./sec.) shown by the followin

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗