Process for producing walking bar members for continuous casting
Abstract
A process for manufacturing a walking bar member for continuous casting from an elongated tubular metal blank by heating the blank at a temperature of 550 DEG to 1250 DEG C., subjecting the heated blank to plastic working which achieves a working ratio of up to 65% or a flattening ratio of over 1 but not greater than 3.0 to flatten the blank into a tubular body by compression over the entire length thereof, and machining a surface of the tubular body at the side thereof to be brought into contact with a slab to smooth the surface and provide a reduced wall thickness, the working ratio and the flattening ratio being represented by (D-H)/Dx100 and W/H, respectively, wherein D is the outside diameter of the blank before the plastic working, H is the minor diameter of the tubular body after the plastic working, and W is the major diameter of the tubular body after the plastic working.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 13.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for producing a walking bar for continuous casting made of steel alloy of low weldability in the form of a flat tube having upper and lower opposed flat surfaces and a hollow interior over the entire length thereof, comprising: heating a tubular metal blank at a temperature of 550° to 1250° C; placing the heated blank between an upper die and a lower die of a press machine wherein a spacer having a height equal to a predetermined dimension to which the blank is to be compressed minus an amount of elastic restoration of the blank is placed between the upper die and the lower die;
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗