Method for manufacturing oxidic sintered nuclear fuel bodies
Abstract
Method for the manufacture of oxidic sintered nuclear fuel bodies by compacting UO 2 -starting powder or a mixture of UO 2 -and PuO 2 starting powder which contains up to 10% by weight rare-earth oxide, especially Gd 2 O 3 , as an additive into blanks and subsequent densification of these blanks by a heat treatment in a sintering atomsphere with reducing action. The UO 2 -starting powder used for compacting has a specific surface in the range of 2 to 4.5 m 2 /g and/or a mean crystallite diameter in the range of 80 nm to 250 nm, and the heat treatment in the sintering atmosphere with reducing action is carried out at a temperature in the range of 1,500° C. to 1,750° C.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 20.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
In a method for the manufacture of oxidic sintered nuclear fuel bodies by compacting UO 2 -starting powder or a mixture of UO 2 and PuO 2 starting powder which contains up to 10% by weight rare-earth oxide as an additive into blanks and subsequent densification of these blanks by a heat treatment in a sintering atmosphere with reducing action, the improvement comprising compacting UO 2 -starting powder which has at least one of the two properties consisting of a specific surface in the range of 2 to 4.5 m 2 /g and a mean crystallite diameter in the range of 80 nm to 250 nm, and carrying o
- Claim 2Depends on #1
Method according to claim 1, wherein the rare earth oxide is Gd 2 O 3 .
- Claim 3Depends on #1
Method according to claim 1
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗