Patents
US 4,512,804 A#4083169 Most CitedExpiredUnited States (USPTO)Utility

Work-hardenable austenitic manganese steel and method for the production thereof

20Forward Citations (#4083169 Global)
0.5/yrCitation Velocity (#17311515 Global)
7.34Citation PageRank (#1771571 Global)
6Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A work-hardenable austenitic manganese steel has a base composition (each in percent by weight) of 0.7 to 1.7 carbon, 5.0 to 18.0 manganese, 0 to 3.0 chromium, 0 to 4.0 nickel, 0 to 2.5 molybdenum, 0.1 to 0.9 silicon, up to 0.1 phosphorus and contains micro-alloying elements of 0.0 to 0.05 titanium, 0.0 to 0.05 zirconium and 0.0 to 0.05 vanadium; the remainder being iron and impurities arising from the melting process. The ratio of carbon to manganese is in the range of 1:4 to 1:14 and the total amount of micro-alloying elements is limited to a range of 0.002 to 0.05 percent by weight. The melt of the base composition is tapped at 1,450° C. to 1,600° C. into a casting ladle in which the micro-alloying elements are added. An ingot is cast, cooled, reheated to austenitization temperatures and quenched.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 20.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A work-hardenable austenitic manganese steel having an elongation at rupture of 10 percent to 80 percent, as measured according to L=5 d or L=10 d, and essentially consisting of, each in percent by weight: 0.7 to 1.7 C 5.0 to 18.0 Mn 0 to 3.0 Cr 0 to 4.0 Ni 0 to 2.5 Mo 0.1 to 0.9 Si up to 0.1 P with the proviso that the carbon-to manganese ratio is between 1:4 and 1:14, and containing an amount of micro-alloying elements in percent by weight: 0.0 to 0.05 Ti 0.0 to 0.05 Zr with the proviso that the sum Ti +Zr is in the range of 0.002 percent by weight to 0.05 percent by weight

  2. Claim 2Depends on #1

    The austenitic manganese steel as defined in claim 1, further including: boron in the range of 0.002 to 0.008 percent by weight.

  3. Claim 3Independent Claim

    The austeniti

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 20 total)

PatentTitleYearCitations
WO 2006/042930 A1Hot-dip coating method in a zinc bath for strips of iron/carbon/manganese steel—21
CN 100,395,370 CMemory alloy fish bolt fastener material for railway and preparation method thereof20080
WO 2024/225991 A1A novel composition of hadfield steel and the production method thereof—0
US 7,556,865 B2Hot-dip coating method in a zinc bath for strips of iron/carbon/manganese steel200910
US 8,636,857 B2Method to obtain a manganese steel alloy20140
WO 2006/061261 A1Method to obtain a manganese steel alloy, and manganese steel alloy thus obtained—1
RU 2,363,756 C2Method of coating steel bar, containing iron, carbon and manganese, through hot galvanising20097
WO 0,233,139 A1Grain-refined austenitic manganese steel casting having microadditions of vanadium and titanium and method of manufacturing—7
CN 102,766,747 BManufacturing method of high-strength non-magnetic abrasion-resistant steel20130
EP 0,904,154 A4Comminuting media comprising martensitic/austenitic steel containing retained work-transformable austenite—0
US 2007292299 A1Method to Obtain a Manganese Steel Alloy, and Manganese Steel Alloy Thus Obtained—0
US 6,572,713 B2Grain-refined austenitic manganese steel casting having microadditions of vanadium and titanium and method of manufacturing20038
US 5,380,483 AVibration-damping alloy19957
US 2008083477 A1Hot-Dip Coating Method in a Zinc Bath for Strips of Iron/Carbon/Manganese Steel—28
US 2023257839 A1A method of casting a steel semi-product with high titanium content—0