Patents
US 4,500,350 A#7453914 Most CitedExpiredUnited States (USPTO)Utility

Disintegration of chromites

13Forward Citations (#7453914 Global)
0.3/yrCitation Velocity (#24791378 Global)
2.87Citation PageRank (#8117619 Global)
5Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

In the disintegration of a chromite or chromium-containing residue, wherein the chromium-containing material is disintegrated with an alkaline compound in the presence of oxygen and a diluent at a temperature above about 800° C. and thereafter leached, the improvement which comprises pre-roasting the chromium-containing material prior to addition of the alkaline compound. Pre-roasting can be effected at 400° to 1200° C. with addition of certain amounts of silica dioxide and/or aluminum oxide and such additives, depending on the chromium containing material, if still required, are added--prior to disintegration and leaching--in such a quantity to establish a ratio of SiO 2 : AL 2 O 3 of about 2:1 and further a ratio, calculated on the basis of NaOH as the alkaline compound, of SiO 2 : Na 2 O of about 1:0.5 plus a Cr 2 O 3 : Na 2 O ratio of about 1:2 to 1:4. Residues from previous leaching cycles can be present during disintegration as solid diluents but their contents of SiO 2 and/or Al 2 O 3 are not taken into account in calculating the SiO 2 :AL 2 O 3 ratios. The process gives excellent results even with starting materials relatively high in SiO 2 which are difficult to disintegra

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 13.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    In the disintegration of a chromite or chromium containing residue, wherein the chromium-containing material is disintegrated with an alkaline compound in the presence of oxygen and a diluent at a temperature above about 800° C. and thereafter leached, the improvements which comprise employing as said chromium-containing material a chromite selected from the group consisting of gangue-rich chemical grade chromite, metallurgical-grade chromite and refractory-grade chromite, and pre-roasting the chromium-containing material for about 2 hours at 1000° to 1100° C. whereby upon subsequent disintegr

  2. Claim 2Depends on #1

    A process as claimed in claim 1, wherein to the chromium-containing material prior to pre-roasting there is added an additive material which contains or is able to form at lea

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • Udy, M. J., Chromium, vol. I, Rheinhold Pub. Corp., p. 265, (1956).