Chemical approach for controlling nadimide cure temperature and rate with maleimide
Abstract
Polyimide resins suitable for use as composite matrix materials are formed by copolymerization of maleic and norbornenyl endcapped monomers and oligomers. The copolymers can be cured at temperatures under about 300 DEG C. by controlling the available concentration of the maleic end-capped reactant. This control can be achieved by adding sufficient amounts of said maleic reactant, or by chemical modification of either copolymer, so as to either increase Diels-Alder retrogression of the norbornenyl capped reactant and/or holding initiation and polymerization to a rate compatible with the availability of the maleic-capped reactant.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 3.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
A composition of the formula: ##STR11## wherein n is an integer of 1 to 20, made by the process comprising increasing the amount of maleic end-capped prepolymer reactant relative to the amount of norbornenyl end-capped prepolymer reactant and copolymerizing the reactants at temperatures under 300° C.
- Claim 2Independent Claim
A composition comprising a mixture of maleic end-capped prepolymer reactant and a norbornenyl end-capped prepolymer reactant capable of copolymerizing at a temperature between 200° C. and 300° C. to yield a polyimide resin essentially of the formula: ##STR12## wherein the norbornenyl end-capped reactant is generated from a mixture of compounds of the formulae: ##STR13## wherein R 1 is a tetravalent aromatic radical and at least two of R 2 are alkyl with the remainder being hydrogen; and H.sub.2 N--R.sub.3 --NH.sub.2
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗