Processed ferrous metal and process of production

7Forward Citations (#15469077 Global)
0.2/yrCitation Velocity (#36072608 Global)
1.67Citation PageRank (#19319063 Global)
12Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Processed low carbon iron metal and process and apparatus for its production, using high water-vapordecarburization, are provided. The iron metal product is characterized by fine grain structure with average carbon content less than about 0.04%. The process is carried out using a cost beneficial protocol including the step of processing scrap steel segments at high density in a strongly decarburizing atmosphere.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 7.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    In the production of ferrous metal from carbon-containing non-particulate scrap steel segments, the steps comprising: establishing in the chamber or retort of an axial flow decarburizing atmosphere furnace a random loaded gas-permeable array of non-particulate scrap steel segments each having a maximum dimension of about eight inches and thus loaded being spatially distributed to accommodate uniform axial gas flow among the segments so as to avoid mobilizing or mixing of the loaded segments during decarburizing; subjecting the thus loaded segments to a decarburizing anneal cycle in a circula

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (1)

  • Metals Handbook, 9th ed. vol. 1, Properties and Selection: Irons and Steels 1978, p. 140.