Patents
US 4,489,110 A#3997728 Most CitedExpiredUnited States (USPTO)Utility

Polyethylene terephthalate moulding compositions having high reflectivity

21Forward Citations (#3997728 Global)
0.5/yrCitation Velocity (#15215905 Global)
2.81Citation PageRank (#8407920 Global)
14Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Polyethylene terephthalate moulding compositions which contain delaminated kaolin may be processed into highly-reflecting objects.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 21.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A process for preparing light reflectors comprising (i) molding an article using a composition comprising (I) from 30 to 85 parts by weight of polyethylene terephthalate having an intrinsic viscosity of at least 0.4 dl/g as measured by using a 0.5%, by weight solution in phenol/o-dichlorobenzene (weight ratio 60:40) at 25° C.: (II) from 2 to 70 parts, by weight, of delaminated kaolin; and (III) from 0 to 70 parts, by weight, of fillers other than delaminated kaolins and/or reinforcing agents and (ii) metallizing at least a portion of said article.

  2. Claim 2Depends on #1

    The process of claim 1 wherein at least 90% by weight of said delaminated kaolin have particle thicknesses of from 0.02 to 0.2 microns.

  3. Claim 3Depends on #1

    The process of claim 1 wherein said delaminated kaolin is characterized in that its average particle thickness is less than 0.1

Technical Overview & Description