Patents
US 4,489,033 A#993105 Most CitedExpiredUnited States (USPTO)Utility

Process for injection compression molding

48Forward Citations (#993105 Global)
1.1/yrCitation Velocity (#5436843 Global)
14.56Citation PageRank (#568105 Global)
2Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A process for injection compression molding ultra high molecular weight polyethylene having an intrinsic viscosity of 3 dl/g or higher measured at 135 DEG C. in decalin and a melt index of 0.01 g/10 min or less comprises, (a) heating the ultra high molecular weight polyethylene to 170 DEG -240 DEG C., (b) adjusting the volume of the mold cavity V1 equal to the volume of the molded article V0, (c) injecting ultra high molecular weight polyethylene having a volume V0 into the mold cavity through a runner portion at a shear rate of at least 20,000 sec-1, (d) instantaneously expanding the mold cavity to adjust its volume V1 to satisfy the relation: 1.2 V0</=V1 at a time from T1 (immediately before completion of injection) and a time T2 (after completion of injection while there is a pressure difference between the cavity and the runner portion, and the ultra high molecular weight polyethylene in the runner portion being solidified), and (e) compressing the volume of the mold cavity V1 to satisfy the relation: V1=V0 while the ultra high molecular weight polyethylene in the mold cavity is still in a molten state.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 48.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for injection compression molding ultra high molecular weight ployethylene having an intrinsic viscosity of at least 3 dl/g measured at 135° C. in decalin and a melt index of up to 0.01 g/10 min which comprises, (a) heating ultra high molecular weight polyethylene to 170°-240° C., (b) adjusting the volume of the mold cavity V 1 in a mold at a mold temperature of from 80° C. to 120° C. to be equal to the volume of the molded article V 0 , (c) injecting ultra high molecular weight polyethylene having volume V 0 into the molded cavity through a runner portion at a shear rate of at

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (2)

Non-Patent Literature (2)

  • SPE Journal, "Injection Stamping--A Special Process for the Production of Large Injection Molded Articles", Apr. 1968, vol. 24, pp. 61-63.
  • SPE Journal, Injection Stamping A Special Process for the Production of Large Injection Molded Articles , Apr. 1968, vol. 24, pp. 61 63.