Method of making class D sucker rods
Abstract
It has been found that API Class D sucker rods can be made inexpensively from low-alloy, low-cost steel by following a suitable induction-normalizing process and using a suitable steel to which there has been added 0.07 to 0.15 percent of vanadium.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 12.
Claims (3 — 2 Independent, 1 Dependent)
- Claim 1Independent Claim
The process of manufacturing a high-strength sucker rod from a carbon steel which comprises heating to a normalizing temperature by means of electric induction an elongated rod of steel suited for the manufacture of a sucker rod, said steel consisting essentially of about: 0.34 to 0.44 percent carbon, 1.35 to 1.65 percent manganese, up to 0.04 percent phosphorus, up to 0.05 percent sulphur, 0.15 to 0.30 percent silicon, 0.07 to 0.15 percent vanadium, balance iron and incidental impurities, and then permitting said rod to cool in air while so supporting and rotating said rod as to p
- Claim 2Depends on #1
A process as defined in claim 1, characterized in that there is thereby produced a sucker rod having an ultimate tensile strength in the range of 115,000 to 140,000 pounds per square inch.
- Claim 3Independent Claim
The
Technical Overview & Description