Method of manufacturing rails
Abstract
At the outlet of a hot rolling mill the temperature of a hot rolled rail is reduced to a value not lower than that at which the pearlitic transformation begins in the rail head. The continuously moving rail is then rapidly cooled to below 650° C. so that at least 80% of the austenite-pearlite transformation has occurred at the end of rapid cooling. The rail is then cooled to ambient temperature.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 14.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of manufacturing rails, comprising the sequential steps of hot rolling a rail in a hot rolling mill; at the outlet of the hot rolling mill, reducing the rail temperature to a value not lower than the temperature at which the pearlitic transformation begins in the rail head; after reaching this temperature, continuously moving the rail and rapidly cooling it to a temperature below about 650° C. so that at least 80% of the allotropic austenite-pearlite transformation has occurred in the rail at the end of rapid cooling; and then cooling the rail to ambient temperature.
- Claim 2Depends on #1
A method as claimed in claim 1, in which the rate of rapid cooling is between 2° C./s and 10° C./s.
- Claim 3Depends on #1
A method as claimed in claim 1, including adjusting the heat transfer coefficient between the rail and the cooling agent during rapid cooling.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (14 of 14 total)
References Cited — Backward Prior Art (2)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 2,882,191 A | Method and apparatus for flame hardening of rails and the like | 1959 | 15 |
| US 3,497,403 A | Surface hardening of rails | 1970 | 4 |