Abstract

In order to increase the crystalline oxide content of barrier layer oxide and hence its capacitance, aluminum electrolytic capacitor foil is anodized at an average current density of at most 3 mA/cm2 of effective surface area in an aqueous electrolyte of C4 to C7 unsubstituted aliphatic dicarboxylic acid containing 0 to 0.05 wt. % of citric acid or tartaric acid and preferably at a temperature above 70 DEG C. The anodized foil is subjected to a relaxation and reanodization treatment to stabilize the foil. The anodization at low current density promotes high crystalline oxide content of the barrier layer oxide, and the relaxation and reanodization insure a stable barrier layer oxide of increased capacitance.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 3 · Forward citations: 53.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A process for increasing the capacitance of anodized aluminum electrolytic capacitor foil by electrolytically anodizing said foil at an average current density between 20 μA and 3 mA per cm 2 of effective surface area in an aqueous electrolyte consisting essentially of an unsubstituted aliphatic dicarboxylic acid containing 0 to 0.05 wt. % of an additive selected from the group of citric acid and tartaric acid to form a barrier layer oxide on said foil having an increased crystalline oxide content, and passing said foil through at least one relaxation and reanodization step to stabilize said

  2. Claim 2Depends on #1

    A process according to claim 1 wherein there are more than one relaxation and reanodization steps and at last of said reanodization steps is carried out in an aqueous phosphate electrolyte.

  3. Claim 3Independent Claim

    A process according t

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 53 total)

PatentTitleYearCitations
US 11,469,052 B2Oxide on edges of metal anode foils20220
US 6,486,530 B1Integration of anodized metal capacitors and high temperature deposition capacitors200238
US 8,206,833 B2Metal oxide film, laminate, metal member and process for producing the same20126
US 7,125,610 B2Capacitor containing aluminum anode foil anodized in low water content glycerine-phosphate electrolyte without a pre-anodizing hydration step20062
US 11,185,948 B2Laser drilling of metal foils for assembly in an electrolytic capacitor20210
US 7,780,835 B2Method of making a capacitor by anodizing aluminum foil in a glycerine-phosphate electrolyte without a pre-anodizing hydration step20100
US 10,825,613 B2Use of etch resist masked anode frame for facilitation of laser cutting, particle and leakage current reduction20200
US 2006124465 A1Capacitor containing aluminum anode foil anodized in low water content glycerine-phosphate electrolyte—0
US 2005103640 A1Method of anodizing aluminum utilizing stabilized silicate solutions—0
US 7,342,773 B2Capacitor containing aluminum anode foil anodized in low water content glycerine-phosphate electrolyte20087
US 12,340,951 B2Laser drilling of metal foils for assembly in an electrolytic capacitor20250
CN 102,839,408 AMethod for preparing porous aluminum oxide film with super-large hole pitch through ultrasonic auxiliary anode oxidation—6
US 5,382,347 AProtective coatings for metal parts to be used at high temperatures199528
US 7,452,473 B1Laser marking of raw aluminum anode foil to induce uniform patterning etching200821
US 2003160290 A1Edge formation process for aluminum solid electrolytic capacitor—0