Abstract

The present invention relates to the production of photothermally crystallizable, chemically-machinable glass-ceramic articles exhibiting coefficients of thermal expansion over the temperature interval of 20°-400° C. between 120-160×10 -7 /° C. Base glass articles having compositions consisting essentially, in weight percent, of 5.5-15% Li 2 O, 2-25% Al 2 O 3 , the weight ratio Al 2 O 3 :Li 2 O being less than 1.7:1, 60-85% SiO 2 , and at least one photosensitive metal in the indicated proportion selected from the group of 0.001-0.03% gold, computed as Au, 0.001-0.3% silver, computed as AgCl, and 0.001-1% copper, computed as Cu 2 O, are first exposed to ultraviolet radiations to develop a latent image therein, then heated to a temperature between the annealing and softening points thereof to generate metallic nuclei therein and the growth of lithium metasilicate particles thereon, and, finally, heated to a temperature in excess of 700° C., but less than 800° C., to effect an essentially crystalline article, including the conversion of a portion of the lithium metasilicate crystals to lithium disilicate. Quartz and/or cristobalite will also be formed.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 102.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A chemically-machinable glass-ceramic exhibiting a coefficient of thermal expansion over the interval of 20°-400° C. of about 120-160×10 -7 /°C. consisting predominantly of lithium metasilicate, lithium disilicate, and quartz and/or cristobalite crystals dispersed in a residual glassy matrix, said glass-ceramic having a composition consisting essentially, expressed in terms of weight percent on the oxide basis, of 5.5-15% Li 2 O, 2-25% Al 2 O 3 , the weight ratio Al 2 O 3 :Li 2 O being less than 1.7:1, 60-85% SiO 2 , and at least one photosensitive metal in the indicated proportion selec

  2. Claim 2Independent Claim

    A chemically-machinable gl