An integrally bladed bimetallic rotor for high temperature operation having airfoils with good stress rupture and creep strength and a hub with high tensile strength and good low cycle fatigue resistance is made from a preform of two concentric cylinders of different superalloy metals metallurgically bonded to each other at their interface, both materials being in such a condition that they exhibit superplastic behavior at a certain, controlled strain rate and temperature without incurring substantial grain growth. The metal of the outer cylinder is selected such that it has a lower gamma prime solvus temperature than the metal of the inner cylinder. The preform is isothermally forged at the controlled strain rate and temperature to form the airfoils from the alloy of the outer cylinder and to form the hub from the alloy of the inner cylinder. A sharp, reproducible interface is created between the two alloys. After forging, the rotor is heated to a temperature between the gamma prime solvus temperatures of the alloys and under conditions which cause full gamma prime solutioning of the airfoils up to the interface but only partial gamma prime solutioning of the rotor hub. The result

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 76.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for fabricating an integrally bladed bimetallic rotor having coarse grained airfoils and an equiaxed fine grained hub portion, comprising the steps of: (1) forming a bimetallic preform having an axis and comprising a first cylinder of a first superalloy metal surrounded by a second cylinder of a second superalloy metal, said second superalloy metal being selected to have a gamma prime solvus temperature at least 25° F. lower than the gamma prime solvus temperature of said first superalloy metal, said step of forming a bimetallic preform including the step of metallurgically bonding s

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗