Patents
US 4,477,427 A#1728820 Most CitedExpiredUnited States (USPTO)Utility

Process for the preparation of alkali-poor α-alumina for ceramic purposes

35Forward Citations (#1728820 Global)
0.8/yrCitation Velocity (#8658282 Global)
9.05Citation PageRank (#1250691 Global)
6Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Process for the preparation of alkali-poor α-alumina for ceramic purposes. Technical grade aluminum hydroxide is activated and calcinated in the presence of a mineralizing mixture comprising halides and boron compounds. The process further comprises activating aluminum hydroxide at a temperature of 500-600 degrees C., washing the activated product with alkali-free water containing calcium ions and having a conductivity not exceeding 70 μS/cm until the alkali content expressed in Na 2 O becomes lower than 0.15% by weight, adding 0.4-0.7% by weight of a mineralizing mixture to the washed product, and calcinating the same at a temperature of 1200-1350 degrees C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 35.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    Process for the preparation of alkali-poor α-alumina for ceramic purposes, comprising (a) activating technical grade aluminum hydroxide by heating it to a temperature of 500°-600° C., (b) washing the activated product with alkali-free water containing calcium ions and having a conductivity not exceeding 70 μs/cm until the alkali content expressed in Na 2 O becomes lower than 0.15% by weight, and (c) calcinating the same in the presence of a mineralizing mixture comprising halides and boron compounds.

  2. Claim 2Depends on #1

    Process according to claim 1, which comprises activating aluminum hydroxide for 10-30 minutes.

  3. Claim 3Depends on #1

    Process according to claim 1, which comprises adding to the washed product as mineralizing mixture 0.3-0.45% by weight of boric acid and 0.1-0.15% by weight of aluminum fluoride, based on the total weight.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 35 total)

PatentTitleYearCitations
US 2006258532 A1Improved alumina carriers and silver-based catalysts for the production of alkylene oxides—19
US 2007111886 A1Catalysts having enhanced stability, efficiency and/or activity for alkylene oxide production—21
US 5,296,085 AMacrocrystalline α-alumina hexagonal platelets199414
US 8,603,937 B2Olefin epoxidation process, a catalyst for use in the process, a carrier for use in preparing the catalyst, and a process for preparing the carrier20133
US 4,623,364 AAbrasive material and method for preparing the same1986539
US 2006293180 A1Modified alumina carriers and silver-based catalysts for the production of alkylene oxides—11
US 8,513,156 B2Catalysts having enhanced stability, efficiency and/or activity for alkylene oxide production20132
US 4,797,270 AMethod for the obtention of an especial alumina from the powder produced in metallurgical alumina calcination198940
US 6,162,413 AAlpha-alumina and method for producing same200022
US 8,536,083 B2Olefin epoxidation process, a catalyst for use in the process, a carrier for use in preparing the catalyst, and a process for preparing the carrier20131
WO 03,055,803 A3Particulate alumina, method for producing particulate alumina and composition containing particulate alumina—0
US 7,528,270 B2Process for the production of an olefin oxide, a 1, 2-diol, a 1,2-diol ether, or an alkanolamine20092
US 5,302,368 AProcess for preparation of alumina199468
WO 2006/028940 A3An olefin epoxidation process, a catalyst for use in the process, a carrier for use in preparing the catalyst, and a process for preparing the carrier—2
US 5,817,588 ACeramic preforms comprising monocrystalline hexagonal platelets of alpha-alumina19984

Non-Patent Literature (2)

  • Gwyra, B. et al., "The Coarsening of Bayer Alumina Trihydrate by Means of Crystallization Modifiers", Powder Technology, 11 No. 2, (1975), pp. 101-105.
  • Gwyra, B. et al., The Coarsening of Bayer Alumina Trihydrate by Means of Crystallization Modifiers , Powder Technology, 11 No. 2, (1975), pp. 101 105.