Patents
US 4,476,236 A#2255838 Most CitedExpiredUnited States (USPTO)Utility

Method for producing a cordierite body

30Forward Citations (#2255838 Global)
0.7/yrCitation Velocity (#10572297 Global)
5.25Citation PageRank (#3061653 Global)
7Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method for producing a cordierite body having no anisotropic property in coefficient of thermal expansion comprises the steps of preparing a raw material containing kaolin mineral and talc as main ingredients, and preformed cordierite particles formed from the raw material, mixing and kneading the raw material together with the preformed cordierite particles into a slurry, forming the slurry into a formed body and firing the formed body.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 30.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for producing a cordierite body comprising the sequential steps of: (1) preparing a first batch material having an average particle diameter of from about 1 to about 50 microns consisting essentially in weight percent of 33.98 to 42.05% kaolin mineral particles, 14.74 to 18.24% raw talc particles, 14.74 to 18.25% fired talc particles produced by delaminating pulverized, layered raw talc along (001) Plane into plate-shaped particles then firing said plate-shaped particles, and at least one of aluminum hydroxide or alumina, the batch material having substantially the same composition ra

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗