Coating compositions and method for the treatment of metal surfaces
Abstract
An aqeuous acidic composition provides improved coating for aluminum. The composition comprises from about 10 to about 150 ppm zirconium, from about 20 to about 250 ppm fluoride, from about 30 to about 125 ppm tannin, from about 15 to about 100 ppm phosphate and from about 5 to about 50 ppm zinc, said coating solution having a tannin to phosphate ratio in the range of at least about 1:1 to about 2:1 and a pH in the range of about 2.3 to about 2.95.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 51.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A non-chromate coating solution effective in forming a coating on aluminum comprising: from about 10 to about 150 ppm zirconium, from about 20 to about 250 ppm fluoride, from about 30 to about 125 ppm tannin, from about 15 to about 100 ppm phosphate and from about 5 to about 50 ppm zinc, said coating solution having a tannin to phosphate ratio in the range of at least about 1:1 to about 2:1 and a pH in the range of about 2.3 to about 2.95.
- Claim 2Depends on #1
A non-chromate coating solution as recited in claim 1 wherein said coating solution is effective in forming a coating to impart corrosion resistance to an aluminum surface, said coating solution comprising from about 40 to about 80 ppm zirconium, from about 50 to about 200 ppm fluoride, from about 40 to about 80 ppm tannin, from about 25 ppm to about 50 ppm phosphate and from about ppm to abou