Aqueous polysiloxane formulations
Abstract
A process for the preparation of an organopolysiloxane composition, comprising polymerizing at a temperature from about room temperature to 250° C. a composition by weight comprising approximately (a) 10 to 90% organopolysiloxane, (b) 4.999 to 85% of at least one of a surfactant and a water-soluble polyether, (c) 85-5% of at least one polymerizable vinyl monomer, and (d) 0.001 to 2% of a radical forming polymerization catalyst, whereby the vinyl monomer is polymerized and forms polymer bridges between (a) and (b). The resulting composition is miscible with and/or readily dispersible in water, is storage-stable and is especially useful as a textile auxiliary.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 20.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
An aqueous emulsion by weight comprising approximately (a) 22 to 99.899% of water, (b) 0.01 to 18% of an emulsifier, and (c) 0.1 to 60% of a composition produced by polymerizing at a temperature from about room temperature to 250° C. a composition by weight comprising approximately (i) 10 to 90% organopolysiloxane, (ii) 4.999 to 85% of at least one of a surfactant and a water-soluble polyether. (iii) 85-5% of at least one polymerizable vinyl monomer, and (iv) 0.001 to 2% of a radical forming polymerization catalyst. whereby the vinyl monomer is polymerized and forms polymer bridges b
- Claim 2Depends on #1
An emulsion according to claim 1, wherein the organopolysiloxane is a diorganopolysiloxane.
- Claim 3Depends on #1
An emulsion according to claim 1, wherein the vinyl monomer comprises at least on member selected from the g
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗