US 4,468,253 A#8985447 Most CitedExpiredUnited States (USPTO)Utility

Method and apparatus for continuously manufacturing non-sintered pellet

11Forward Citations (#8985447 Global)
0.3/yrCitation Velocity (#27907079 Global)
2.97Citation PageRank (#7685773 Global)
4Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method and an apparatus for continuously manufacturing a non-sintered pellet, which comprises: continuously supplying a green pellet having a water content of from 6 to 20 wt. % into a shaft type reactor to continuously pass the green pellet sequentially through a pre-treating zone, a hydration reaction zone and a drying zone in the shaft type reactor; blowing a pre-treating gas with a relative humidity of up to 70% and at a temperature of from 65° to 250° C. into the pre-treating zone to pre-dry the green pellet in the pre-treating zone until the difference in the water content in the green pellet before and after the abovementioned pre-drying becomes at least 4 wt. % within the limits in which the green pellet in the pre-treating zone contains at least 2 wt. % water; blowing a gas for hydration reaction at a temperature of from 50° to 100° C. containing saturated steam into the hydration reaction zone to hydrate the green pellet in the zone; and, blowing a drying gas at a temperature of from 100° to 300° C. into the drying zone to dry the green pellet in the zone, thereby hardening the green pellet in the drying zone to continuously manufacture a non-sintered pellet.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 11.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for continuously manufacturing a non-sintered pellet, which comprises: adding a hydraulic binder and water to raw materials which comprise at least one of an iron ore fine, a non-ferrous ore fine and a dust mainly containing oxides of iron or non-ferrous metal, and mixing same; forming the resultant mixture to prepare a green pellet having a water content within the range of from 6 to 20 wt. %; continuously supplying said green pellet into a shaft type reactor which comprises a pre-treating zone, a hydration reaction zone following said pre-treating zone and a drying zone following sa