Sinterable fluorite oxide ceramics
Abstract
Zirconia ZrO 2 , ceria CeO 2 or thoria ThO 2 may be rendered ionically conductive; a typical composition is ZrO 2 +12 mol % CaO. This is sintered in the solid state as a 40 nm powder using as a sintering additive 0.1 mol % MgO at 1450 C. for 4 hours; a density 98% of the theoretical is achieved. For other fluorite oxide compositions, MgO is also useful as a sintering additive but in different proportions.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 19.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A composition of fluorite oxide sinterable in the solid state, comprising a fluorite oxide, which may be partly or fully stabilised, characterised in that it contains 0.05 to 0.15 mole % MgO and substantially no Al 2 O 3 .
- Claim 2Depends on #1
A composition according to claim 1, wherein the particle size of the fluorite oxide does not exceed 1 micron.
- Claim 3Depends on #2
A composition according to claim 2, wherein the said particle size does not exceed 0.4 micron.