Abstract

Disclosed is a method of preparing a clear partially hydrolyzed aluminum alkoxide solution by mixing an aluminum alkoxide with about 0.4 to about 1 moles of water per mole of aluminum alkoxide in the presence of sufficient alcohol to give a maximum weight percent of equivalent alumina of 10%. The mixture is then heated until clear, which typically requires a temperature of about 40 DEG to about 60 DEG C. Then sufficient additional water is added to bring the number of moles of water per mole of alkoxide up to at least about 2. The water is added in the presence of sufficient alcohol to give a maximum weight percent of equivalent alumina of about 3%. A polymerized alumina glass can be prepared from the composition by heating it to a temperature of at least 500 DEG C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 6.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of forming a polymerized Al 2 O 3 coating on a substrate comprising preparing a clear partially hydrolyzed aluminum alkoxide solution by (A) mixing Al(OR) 3 with about 0.4 to about 1 mole of water per mole of Al(OR) 3 in the presence of sufficient alcohol to give a maximum weight % of equivalent Al 2 O 3 of 10% where R is alkyl to C 6 ; (B) applying said solution to a surface of a substrate; and (C) heating said solution on said surface to at least about 400° C.

  2. Claim 2Depends on #1

    A method according to claim 1 including the additional last step of adding sufficient additional water to bring the number of moles of water per mole of alkoxide up to at least about 2, in the presence of sufficient alcohol to give a maximum weight % of equivalent Al 2 O 3 of about 3%.

  3. Claim 3Depends on #1

    A method according to claim 1 wherein R is seconda

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (2)